Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 61.0 °C | 142 °F | of Solvent |
3M Novec™ 1710 Electronic Grade Coating 3M™ Novec™ 1710 Electronic Grade Coating is a higher solids version of Novec™ 1700. It is a clear, low viscosity, low surface tension solution of a 10 wt% fluorochemical acrylic polymer carried i.. |
|||
Boiling Point | 61.0 °C | 142 °F | |
3M Novec™ 7100DL Engineered Fluid A higher purity version of 3M™ Novec™ 7100, 3M™ Novec™ 7100DL is tightly-controlled for ions, metals and non-volatile residue. It is used in precision cleaning and deposition applications when h.. |
|||
Boiling Point | 61.0 °C | 142 °F | of Solvent |
3M Novec™ 1700 Electronic Grade Coating 3M™ Novec™ 1700 Electronic Grade Coating is designed for the protection of printed circuit boards and electronic components. It is a clear, low viscosity solution of a 2 wt% fluorochemical acrylic.. |
|||
Boiling Point | 61.0 °C | 142 °F | of Solvent |
3M Novec™ 1720 Electronic Grade Coating 3M™ Novec™ 1720 Electronic Grade Coating adds easy clean capabilities to surfaces such as glass flat panel displays and mobile electronic device components. It is a clear, 0.1 wt% fluorosilane pol.. |
|||
Boiling Point | 61.0 °C | 142 °F | of Solvent |
3M Novec™ 1702 Electronic Grade Coating 3M™ Novec™ 1702 Electronic Grade Coating is a lower solids version of Novec™ 1700. It is a clear, low viscosity, low surface tension solution of a 0.2 wt% fluorochemical acrylic polymer carried i.. |
|||
Boiling Point | 61.0 °C | 142 °F | |
3M Novec™ 7100 Engineered Fluid 3M™ Novec™ 7100 Engineered Fluid, methoxy-nonafluorobutane (C4F9OCH3), is a clear, color less and low-odor fluid intended to replace ozone-depleting substances (ODSs) and compounds with high globa.. |
|||
Boiling Point | 61.0 °C | 142 °F | |
3M Novec™ 71IPA Engineered Fluid 3M™ Novec™ 71IPA Engineered Fluid is ideal for light cleaning and degreasing tasks. 3M™ Novec™ 71IPA has essentially constant vapor and liquid composition at its boiling point. Excellent replace.. |