Thermal Properties Metric English Comments
Boiling Point 79.0 °C
174 °F
of Solvent
3M Novec™ 2708 Electronic Grade Coating
3M™ Novec™ 2708 Electronic Grade Coating is designed for the protection of printed circuit boards and electronic components. It is a low viscosity solution of a 8 wt% fluorochemical acrylic polyme..