Thermal Properties Metric English Comments
Boiling Point 95.0 °C
203 °F
Solvay Chemicals 2,2-Difluoroethanol
CAS-No.: 359-13-7 Uses: Chemical industry, Chemical intermediate and Laboratory chemicalsInformation provided by Solvay
Boiling Point 95.0 °C

@Pressure 0.101 MPa
203 °F

@Pressure 14.7 psi
3M Fluorinert™ FC-770 Electronic Liquid
3M™ Fluorinert™ Liquid FC-770 is a non-conductive, thermally and chemically stable fluid with a wide liquid range (-125 to 95 deg C) for use in many low temperature heat transfer application such ..
Boiling Point 95.0 °C
203 °F
BASF Glutaraldehyde 50% Solution
Formula: C5H8O2CAS: 111-30-8Description: Glutaraldehyde 50% is a colorless to yellow liquid, with a pungent odor. It is also miscible with water.Synonyms: Glutaraldehyde, Pentanedial, 1,5-Pentandia..