Flash Point 276 °C
529 °F
ASTM D92
ChevronTexaco ISO 320 Industrial Oil EP
FeaturesChevron Industrial Oils EP are multipurpose oils for industrial service.Chevron Industrial Oils EP are designed to help minimize wear in all types of plant lubrication and also provide long ..
Flash Point 276 °C
529 °F
ASTM D92
ChevronTexaco NLGI 2 Moly MAX Grease EP
FeaturesChevron Moly MAX Greases EP are high performance greases.They are formulated with extreme pressure additives and 5% molybdenum disulfide (moly). They are dark gray/black in color and smooth ..
Flash Point 276 °C
529 °F
ChevronTexaco Regal® AW 100
Texaco Regal AW oil delivers value through:High Temperature stability provides long lubricant life and resistance to formation of sludge and varnish on bearings and gears.Excellent wear protection p..
Flash Point 276 °C
529 °F
[°C] Fire Point
ChevronTexaco Canopus® 68
Texaco Canopus oils deliver value through:High resistance to forming emulsions due to excellent water separating characteristics.Long lubricant life provided by outstanding stability.Good lubricant ..
Flash Point 276 °C
529 °F
ASTM D92
ChevronTexaco Clarity® ISO 100 Paper Machine Oil
FeaturesChevron Clarity Paper Machine Oils are the next generation circulating oils for the pulp and paper industry.Chevron Clarity Paper Machine Oils ISO 100, 150, and 220 are formulated with ISOS..
Flash Point 276 °C
529 °F
3M Scotch-Weld™ 6111HT Blue Bulk only Adhesive
Same as 6111 but has higher heat resistance and blue in colorInformation provided by 3M
Flash Point 276 °C
529 °F
3M Scotch-Weld™ 6111HT Tan Bulk only Adhesive
Same as 6111 but has higher heat resistanceInformation provided by 3M