Polymer Property : Flash Point = 1.67 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 1.67 °C
35.0 °F
Lord Adhesives AP-134 Reactive Polymer Primer or Adhesive for Polar Substrates
Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa..