Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 108 °C | 226 °F | ASTM D92 |
ExxonMobil Mobil Aero HFA Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |
|||
Flash Point | 108 °C | 226 °F | ASTM D92 |