Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 11.0 °C | 51.8 °F | Seta |
Lord Adhesives Chemlok® Y-1520A Adhesive LORD Chemlok® Y-1520A adhesive is a clear, one-coat adhesive used to bond specialty elastomers to metal and plastics during vulcanization of the rubber. Chemlok Y-1520A adhesive is useful for bon.. |
|||
Flash Point | 11.0 °C | 51.8 °F | closed cup |
Lucite International Colacryl ® TS1173 Reactive Acrylic Syrup Lucite® Colacryl® TS1173 is a reactive polymer solution containing dissolved polymers, plasticiser and a polymerisation activator.Information provided by Lucite International |
|||
Flash Point | 11.0 °C | 51.8 °F | Seta |
LyondellBasell TEBOL® 99 High Purity TBA, Tertiary butyl alcohol Information provided by Lyondell. |
|||
Flash Point | 11.0 °C | 51.8 °F | |
Indium Corp. Indalloy® 84004 Flux #4-0A Clear Liquid Flux Indalloy Flux #4-0A is a clear liquid flux formulated for the purpose of soldering moderately easy to difficult metallizations such as nickel, oxidized copper, Kovar and brass. This flux contains o.. |
|||
Flash Point | 11.0 °C | 51.8 °F | closed cup |
Dow Corning 1-6136 ANTISTAT Dow Corning 1-6136 Antistat is a cationic alkoxy silane and is designated 3-trimethoxysilylpropyloctadecyidimethyl ammonium chloride. It is supplied as a 42 percent active solution (by weight) in me.. |
|||
Flash Point | 11.0 °C | 51.8 °F | |
BASF 1,4-Dioxane Formula: C |
|||
Flash Point | 11.0 °C | 51.8 °F | |
BASF 1,4-Dioxane stab Formula: C4H8O2CAS: 123.91.1Description: 1,4-Dioxane stab. is a colorless to yellow liquid, with an ether-like odor. It is miscible with water and other organic solvents. Synonyms: p-Dioxan, Dioxan.. |