Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 50.0 °C | 122 °F | ASTM D93 |
ExxonMobil Solvesso™ 100 Aromatic Fluid Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil |