Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 136 °C | 276 °F | Method A; ASTM D93 |
ExxonMobil Exxsol™ D140 Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Flash Point | 136 °C | 277 °F | |
BASF 1,5-Pentanediol (PDO) Formula: C5H12O2CAS: 111-29-5Description: 1,5-Pentanediol (PDO) is a colorless, oily liquid with characteristic odor. It is miscible in water and organic solvents.Synonyms: 1,5-Dihydroxypentane, 1,5.. |