Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 138 °C | 280 °F | |
Heatbath/Park #50 Oil Quench Low viscosity quench oil that approaches water in quench speed, yet gives a more uniform, less severe quench than water. Recommended for open quench system operating below 120°C.Information provi.. |
|||
Flash Point | 138 °C | 280 °F | closed cup |
Dow Corning Z-6030 SILANE Dow Corning® Z-6030 Silane is a bifunctional silane containing a methacrylate reactive organic group and a trimethoxysilyl inorganic group. The product is designated ?- methacryloxypropyltrimethoxy.. |
|||
Flash Point | 138 °C | 280 °F | closed cup |
Dow Corning 217 FLAKE RESIN Resin binder for powder or liquid coatings or co-binder with organic resins to improve heat stability and weatherability.Information provided by Dow Corning |
|||
Flash Point | 138 °C | 280 °F | closed cup |
Dow Corning 220 FLAKE RESIN Resin binder powder coating binder or co-binder to improve heat stability and weatherability; for blending with other silicone resins to reduce VOC content; in solvent-based organic coatings to impr.. |
|||
Flash Point | 138 °C | 280 °F | closed cup |
Dow Corning 233 FLAKE RESIN Used as a powder coating binder or co-binder to improve heat stability and weatherability; colored baking enamels, decorative finishes; to increase hardness of other liquid silicone resins.Informati.. |
|||
Flash Point | 138 °C | 280 °F | closed cup |
Dow Corning 249 FLAKE RESIN Used as a powder coating binder or co-binder to improve heat stability and weatherability; for blending with solvent-based silicone resins to reduce VOC's; for blending with solvent-based organic re.. |
|||
Flash Point | 138 °C | 280 °F | |
BASF DTD Amine Formula: C26H55NCAS: 900169-60-0Description: Ditridecylamine mixture of isomers is a colorless to yellow liquid with an amine-like odor. It is not miscible with water.Synonyms: 2-Imidazoleidinane, .. |
|||
Flash Point | 138 °C | 280 °F | |
BASF 2-Pyrrolidone Distilled Formula: C4H7NOCAS: 616-45-5Description: 2-Pyrrolidone Distilled is a colorless to yellow liquid, with a faint amine-like odor. It is miscible in water.Synonyms: 2P, Pyrrolidone, 2-Pyrrolidinone, 2-.. |