Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 186 °C | 367 °F | ASTM D92 |
ExxonMobil Mobil Zerice 100 S Oil Mobil Zerice S Oils are premium quality synthetic refrigeration compressor lubricants. Based on alkyl benzenes, which due to their nature, have superior miscibility with hydrochlorofluorocarbon (R2.. |
|||
Flash Point | 186 °C | 367 °F | open cup |
Dow Corning SZ-1346E Silicone Surfactant Dow Corning® SZ-1346E Additive is a non-hydrolyzable silicone surfactant recommended for production of high-resiliency molded PU foam.Information provided by Dow Corning |
|||
Flash Point | 186 °C | 367 °F | |
ChevronTexaco Cepheus® 68 Texaco Cepheus oil deliver value throughThe ability to retain lubrication properties in the presence of water.Good rust protection from a carefully designed additive package.The ease with which they.. |
|||
Flash Point | 186 °C | 367 °F | ASTM D92 |
ChevronTexaco ISO 22 Utility Oil LVI FeaturesChevron Utility Oils LVI are general purpose lubricants. Chevron Utility Oils LVI are light-colored oils that possess excellent natural low pour points, along with low carbon-forming tendenc.. |
|||
Flash Point | 186 °C | 367 °F | ASTM D92 |
ChevronTexaco Mechanism LPS® ISO 46 Hydraulic Oil Chevron Mechanism LPS Hydraulic Oils are highly refined, paraffinic oils containing oxidation and rust inhibitors, and special antiwear additives to extend the life of hydraulic pumps and motor part.. |
|||
Flash Point | 186 °C | 367 °F | ASTM D92 |
ExxonMobil Mobil Zerice 100 S Oil Mobil Zerice S Oils are premium quality synthetic refrigeration compressor lubricants. Based on alkyl benzenes, which due to their nature, have superior miscibility with hydrochlorofluorocarbon (R2.. |
|||
Flash Point | 186 °C | 367 °F | |
ChevronTexaco Alcaid® 19 Texaco Alcaid® oils deliver value through:Low pour points that permit oils to remain fluid at subzero temperatures.Ready separation from water, an important property where severe moisture condition.. |
|||
Flash Point | 186 °C | 367 °F | |
ChevronTexaco Rando® HDZ 46 Texaco Rando HDZ oils deliver value through:High oxidation stability — Longer service life than attainable with conventional lubricants used in high pressure service.Protection against rust and cor.. |