Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 98.9 °C | 210 °F | |
Lubriplate Flush Pure USP Mineral Oil-Based Food Machinery Grade Oil This lubricating, flushing and cleansing oil is to be used along with the existing lubricant to clean equipment without dismantling. It can be used to clean and flush bearings, gear cases, hydraulic.. |
|||
Flash Point | 99.0 °C | 210 °F | |
Solvay CATAFOR® MS/T Surfactant Description: Proprietary blendIdentification: ALKALI METAL SALT IN SOLVENTSoluble in polar organic solvent. Soluble in water.pH: NeutralAvailable in: Asia Pacific, Europe, Latin America and North Am.. |