Thermal Properties Metric English Comments
Flash Point 219 °C
426 °F
ExxonMobil 100 Exxon Sawguide Oil
EXXON SAWGUIDE OIL is specifically formulated to lubricate the thin saw blades of modern gang saws and edgers. The choice of viscosity grade depends on equipment type, lubricant delivery system desi..
Flash Point 219 °C
426 °F
ASTM D92
ChevronTexaco ISO 220 Marine Oil E
FeaturesChevron Marine Oils E are formulated using a blend of high grade, medium viscosity index base oils and carefully balanced additive package to meet the crankcase need of marine steam engines...
Flash Point 219 °C
426 °F
ASTM D92
ChevronTexaco RPM® SAE 10W Heavy Duty Motor Oil
Features: Chevron RPM Heavy Duty Motor Oils are premium quality, mixed fleet motor oils meeting the performance requirements of all four-stroke gasoline engines and all naturally aspirated, turbocha..
Flash Point 219 °C
426 °F
ASTM D92
ChevronTexaco Torque Fluid
Chevron Torque Fluid is a high performance hydraulic fluid designed for use in transmissions and hydraulic systems requiring a fluid meeting the Allison C4 specificationIt is manufactured using high..
Flash Point 219 °C
426 °F
ChevronTexaco URSA® SAE 10W Super Plus
Texaco Ursa Super Plus oils deliver value through:Oil lasts longer between drains — Good oxidation stability protects against oil thickening during manufacturers recommended oil drain periods.Vital..
Flash Point 219 °C
426 °F
ExxonMobil 100 Exxon Sawguide Oil
EXXON SAWGUIDE OIL is specifically formulated to lubricate the thin saw blades of modern gang saws and edgers. The choice of viscosity grade depends on equipment type, lubricant delivery system desi..
Flash Point 219 °C
426 °F
ChevronTexaco URSA® SAE 10W Extra Duty
Texaco Ursa Extra Duty oils deliver value through:Excellent high temperature deposit control. Protects against high temperature oxidation and oil thickening.Special extreme pressure antiwear propert..