Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 104 °C | 220 °F | |
ConocoPhillips SynXPA® HC-150 H Lubricant HC-150 Description: Conoco SynXPA H Lubricant is a premium-quality synthetic-polyolester lubricant that offers protection for heavily loaded and partially opened open gears, such as those in ball mills, sh.. |
|||
Flash Point | 104 °C | 220 °F | |
ConocoPhillips SynXPA® HC-450 H Lubricant HC-450 Description: Conoco SynXPA H Lubricant is a premium-quality synthetic-polyolester lubricant that offers protection for heavily loaded and partially opened open gears, such as those in ball mills, sh.. |