Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 234 °C | 453 °F | ASTM D92 |
ExxonMobil 27 Mobil Mist Lube Series Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig.. |
|||
Flash Point | 234 °C | 453 °F | ASTM D92 |
ExxonMobil Mobil 1 0W-30 Mobil 1 W-30 is an advanced high performance synthetic engine oil designed to provide outstanding wear protection and enhanced fuel economy performance. Mobil 1 0W-30 exceeds the requirements of the.. |
|||
Flash Point | 234 °C | 453 °F | |
ExxonMobil Mobil Turbo 319A-2 Mobil Turbo 319A-2 is a fully synthetic lubricant developed to meet the performance requirements of Russian gas turbine aircraft engines which operate on mineral-oil-based lubricants. Formulated fro.. |
|||
Flash Point | 234 °C | 453 °F | ASTM D92 |
ChevronTexaco FM ISO 46 Lubricating Oil Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr.. |
|||
Flash Point | 234 °C | 453 °F | ASTM D92 |
ChevronTexaco Supreme SAE 10W-40 Motor Oil FeaturesChevron Supreme Motor Oils are premium quality automotive engine oils.Chevron Supreme Motor Oils SAE 5W-20, 5W-30, 10W-30, 10W-40, and 20W-50 are formulated with ISO-SYN™ base stocks, a she.. |
|||
Flash Point | 234 °C | 453 °F | |
ChevronTexaco Texglass MV Texaco Texglass MV delivers value through:Ability to maintain film thickness — High viscosity index indicates an oil that maintains film thickness at high temperatures.Sludge protection — Detergen.. |
|||
Flash Point | 234 °C | 453 °F | ASTM D92 |
ExxonMobil 27 Mobil Mist Lube Series Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig.. |
|||
Flash Point | 234 °C | 453 °F | ASTM D92 |
ExxonMobil Mobil 1 0W-30 Mobil 1 W-30 is an advanced high performance synthetic engine oil designed to provide outstanding wear protection and enhanced fuel economy performance. Mobil 1 0W-30 exceeds the requirements of the.. |
|||
Flash Point | 234 °C | 453 °F | |
ExxonMobil Mobil Turbo 319A-2 Mobil Turbo 319A-2 is a fully synthetic lubricant developed to meet the performance requirements of Russian gas turbine aircraft engines which operate on mineral-oil-based lubricants. Formulated fro.. |
|||
Flash Point | 234 °C | 453 °F | ASTM D92 |
ExxonMobil Nuto 68 H Series Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q.. |
|||
Flash Point | 234 °C | 453 °F | COC |
ConocoPhillips Conoco® El Mar® Mid Ash Heavy Duty SAE 30 Conoco® El Mar Mid Ash Heavy Duty is a high-quality, mid-ash, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately to highly turbocharged 4-stroke cycle natura.. |
|||
Flash Point | 234 °C | 453 °F | COC |
ConocoPhillips Hydroclear Diamond Class® 46 Turbine Oil Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p.. |
|||
Flash Point | 234 °C | 453 °F | ASTM D92 |
ChevronTexaco Vistac® ISO 220 Way Oil FeaturesChevron Way Oils Vistac provide extreme pressure and antiwear protection and have stringiness and oiliness characteristics. As indicated by part of the name, Vistac, these lubricants have an.. |
|||
Flash Point | 234 °C | 453 °F | ASTM D92 |
ExxonMobil 524 Mobil SHC 500 Series Mobil SHC 500 Series oils are supreme performance hydraulic oils formulated from synthesised, wax-free hydrocarbon base fluids combined with a carefully engineered super-stabilised additive system. .. |
|||
Flash Point | 234 °C | 453 °F | |
BASF D 2000 Polyetheramine Formula: C5H9ClOCAS: 9046-10-0Description Polyetheramine D 2000 is a yellowish liquid, with an amine-like odor. It is partly miscible with water and other solvents. Synonyms: Polyetheramine D2000, .. |
|||
Flash Point | >= 234 °C | >= 453 °F | |
BASF Polyetheramine D 2000 Description: Polyethermine D 2000 is a yellowish liquid, with an emine-like odor. It is partly miscible with water and other solvents.Applications: Intermediate used in the production of: Plastics, .. |
|||
Flash Point | 234 °C | 453 °F | |
ConocoPhillips HD Fleet™ 30 Engine Oil Description: Conoco HD Fleet Engine Oil is a high-quality, single-grade oil formulated from Conoco's premium hydrocracked base stock and unique additive technology. This oil is highly recommende.. |
|||
Flash Point | 234 °C | 453 °F | ASTM D92 |
ExxonMobil Nuto 68 H Series Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q.. |
|||
Flash Point | 234 °C | 453 °F | ASTM D92 |
ExxonMobil 524 Mobil SHC 500 Series Mobil SHC 500 Series oils are supreme performance hydraulic oils formulated from synthesised, wax-free hydrocarbon base fluids combined with a carefully engineered super-stabilised additive system. .. |
|||
Flash Point | 234 °C | 453 °F | |
ChevronTexaco Havoline® SAE 10W-30 Synthetic Blend Motor Oil Havoline Synthetic Blend Motor Oil is formulated with a combination of synthetic and premium quality conventional base oils and an advanced additive package.Havoline Synthetic Blend Motor Oil is rec.. |
|||
Flash Point | 234 °C | 453 °F | |
ChevronTexaco Havoline® SAE 10W-40 Motor Oil All grades of Havoline Motor Oils are formulated with high quality base stocks, a shear-stable viscosity index improver, and contain detergent, dispersant, wear control, antioxidant, corrosion inhib.. |