Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | -3.89 °C | 25.0 °F | |
Lord Adhesives 7701 Ethyl Acetate Surface Conditioner Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa.. |
|||
Flash Point | -3.89 °C | 25.0 °F | ASTM D56 |
ExxonMobil MEK Methyl Ethyl Ketone Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil |