Polymer Property : Flash Point = 28.2 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 28.2 °C
82.8 °F
Dow Corning QP8-5314 INTERMEDIATE
Dow Corning QP8-5314 Intermediate was developed specifically as an intermediate for upgrading the weatherability of acrylic emulsions. However, it should work equally well with other emulsion system..