Thermal Properties Metric English Comments
Flash Point 144 - 146 °C
291 - 295 °F
Closed Cup
Solvay RHODISOLV® PORLARCLEAN Solvent
Description: Rhodiasolv PolarClean is a eco-friendly water soluble polar solvent or co-solvent very effective to solubilize agrochemicals. It is recommended to use in EC’s (emulsifiable concent..