Polymer Property : Flash Point = 31.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 31.0 °C
87.8 °F
Permabond Nitroethane Solvent for Cyanoacrylate
The PERMABOND SOLVENT is extremely effective for dissolving cyanoacrylate bonds or removing cured excess adhesive. It is not recommended for use on acrylic plastics. The solvent base is Nitroethane...
Flash Point 31.0 °C
87.8 °F
closed cup
Dow Corning P5200 ADHESION PROMOTER, CLEAR
Dow Corning P5200 Adhesion Promoter is typically applied in a very thin layer to non-porous and porous construction finishes to increase the bonding capacity of Dow Corning silicone construction sea..
Flash Point 31.0 °C
87.8 °F
closed cup
Dow Corning P5200 ADHESION PROMOTER, RED
Dow Corning P5200 Adhesion Promoter is typically applied in a very thin layer to non-porous and porous construction finishes to increase the bonding capacity of Dow Corning silicone construction sea..