Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 330 °C | 626 °F | ASTM E138 |
Plastic Lumber from the Plastic Lumber Co. Description: Plastic Lumber is a product similar to wood that is made from recycled plastic jugs. Products will never splinter, rot, crumble or need painting. Plastic Lumber has rapidly gained accep.. |