Flash Point 166 °C
331 °F
ASTM D92
ChevronTexaco ISO 22 CP Oil
FeaturesChevron CP Oil is used for both cotton picker spindle lubrication and as a corrosion (rust) preventative on steel materials in the steel industry.It is manufactured form medium viscosity ind..