Polymer Property : Flash Point = 338 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point >= 170 °C
>= 338 °F
in closed cup
Kazanorgsintez Polyethyleneglycol, Dust Controller
Production Method: Obtained by interaction of ethylene glycol and ethylene oxide. Application: Used as a reagent in production of potash fertilizers to reduce dust formation.Information Provided by ..
Flash Point 170 °C
338 °F
Solvay STANNINE® 5525 Surfactant
Description: Blend of substituted thiourea and surfactantsIdentification: ACID PICKLING INHIBITOR (SUBSTITUTED THIOUREA)CAS: 61791 – 00 – 2Solubility: Complete in acidsAvailable in: Asia P..
Flash Point 170 °C
338 °F
ASTM D93, DIN 51 755
Chesterton 390 Cutting Oil
Description: Chesterton® 390 Cutting Oil is a heavy duty, multi-purpose cutting fluid designed to provide maximum tool life and superior parts finish in severe applications. It is a highly reinforc..
Flash Point 170 °C
338 °F
Chesterton OPTICOOL™ 372 Lubrication
Description: OPTICOOL 372 is a proven, universal, water miscible metal working fluid. It is ideal where lubricity is important and operations severe. The 372 is suitable for a broad range of metal c..
Flash Point 170 °C
338 °F
PMCC; ASTM D92
ExxonMobil Exterex™ A34 Synthetic Fluid
Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low vol..
Flash Point >= 170 °C
>= 338 °F
Unipetrol Light Oil Hydrogenate
Oil hydrogenates are a fraction boiling at above approximately 300°C, gained from crude oil through distillation and mild hydrocracking. They are a mixture of light colour hydrocarbons of semi-soli..