Polymer Property : Flash Point = 34.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 34.0 °C
93.2 °F
closed cup
Dow Corning OS-20
Information provided by Dow Corning
Flash Point 34.0 °C
93.2 °F
BASF 1,2-PDA 1,2-Propylenediamine
Formula: C3H10N2CAS: 78-90-0Description: 1,2-Propylenediamine is a colorless liquid, with an amine-like odor. It is also miscible with water in all proportionsSynonyms: 1,2-PDA, 1,2-Propanediamine,..
Flash Point 34.0 °C
93.2 °F
BASF N-Methylpiperazine
Formula: C5H12N2CAS: 109-01-3Description: N-Methylpiperazine is a colorless to yellow liquid with an amine-like odor. It is miscible in water. Synonyms: 1-Methylpiperazine, N-MethylpiperazinApplica..