Thermal Properties Metric English Comments
Flash Point 176 °C
349 °F
ASTM D92
ExxonMobil 424 Mobilmet 400 Series
Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operation..
Flash Point 176 °C
349 °F
ASTM D92
ExxonMobil Thermrex Series V-32
The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and ..
Flash Point 176 °C
349 °F
ASTM D92
ChevronTexaco RPM® NLGI 1 Arctic Grease
Chevron RPM Arctic Grease is a premium quality grease.It is manufactured using a polyurea acetate complex thickener, special low viscosity base oil, and rust and oxidation inhibitors. It is black in..
Flash Point 176 °C
349 °F
ASTM D92
ExxonMobil 424 Mobilmet 400 Series
Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operation..
Flash Point 176 °C
349 °F
ASTM D92
ExxonMobil Thermrex Series V-32
The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and ..