Polymer Property : Flash Point = 360 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point >= 182 °C
>= 360 °F
Open Cup (D92)
Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid
Paratherm GLT™ Heat Transfer Fluid is an alkylated aromatic based heat transfer fluid formulated for closed loop liquid phase heating systems to 550°F using fired heaters and to 575°F in waste-he..
Flash Point 182 °C
360 °F
ASTM D92
ExxonMobil LL Mobiltac Double Letter Series
The Mobiltac Double Letter Series products are high performance, non-diluent type, heavy-bodied products intended for the lubrication of open gears over a wide range of environmental conditions and ..
Flash Point 182 °C
360 °F
ASTM D92
ExxonMobil MM Mobiltac Double Letter Series
The Mobiltac Double Letter Series products are high performance, non-diluent type, heavy-bodied products intended for the lubrication of open gears over a wide range of environmental conditions and ..
Flash Point >= 182 °C
>= 360 °F
ASTM D92
ExxonMobil Mobilarma 522
Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The..
Flash Point 182 °C
360 °F
ASTM D92
ChevronTexaco 8-T White Oil
FeaturesChevron White Oils are technical grade oils processed from paraffinic oil. Mixtures of paraffinic and naphthenic hydrocarbons, they are virtually free of nitrogen, sulfur, oxygen, and aroma..
Flash Point 182 °C
360 °F
ASTM D92
ChevronTexaco Elite-Cut® AXH Metal Working Fluid
FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met..
Flash Point 182 °C
360 °F
ChevronTexaco Extra Cutting Oil
Texaco Extra Cutting Oil delivers value through:Excellent metal wetting and lubricity properties that allow the oil to spread rapidly on the metal surface and reduce friction and the chip-tool inter..
Flash Point 182 °C
360 °F
ASTM D92
ChevronTexaco Packers Oil
Flash Point 182 °C
360 °F
ASTM D92
ChevronTexaco Superla® 7 White Oil
FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch..
Flash Point 182 °C
360 °F
ASTM D92
ExxonMobil LL Mobiltac Double Letter Series
The Mobiltac Double Letter Series products are high performance, non-diluent type, heavy-bodied products intended for the lubrication of open gears over a wide range of environmental conditions and ..
Flash Point >= 182 °C
>= 360 °F
ASTM D92
ExxonMobil Mobilarma 522
Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The..
Flash Point >= 182 °C
>= 360 °F
Dow SPECTRIM™ 35A Isocyanate
SPECTRIM™ 35A reaction moldable polymer is one component (SPECTRIM™ 35B-S is the other) of a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology dev..
Flash Point >= 182 °C
>= 360 °F
Dow SPECTRIM™ 50A Isocyanate
SPECTRIM™ 50A reaction moldable polymer is one component (SPECTRIM™ 35A is the other) of a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology devel..
Flash Point 182 °C
360 °F
ConocoPhillips Hydroclear® 70 Industrial Oil
Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende..
Flash Point 182 °C
360 °F
ConocoPhillips Hydroclear® 90 Industrial Oil
Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende..
Flash Point 182 °C
360 °F
ASTM D92
ExxonMobil MM Mobiltac Double Letter Series
The Mobiltac Double Letter Series products are high performance, non-diluent type, heavy-bodied products intended for the lubrication of open gears over a wide range of environmental conditions and ..
Flash Point 182 °C
360 °F
ConocoPhillips 32 Spectrum Cutting Oil
Description: Conoco Spectrum Cutting Oil is a multifunctional cutting fluid formulated with a sulfurized base oil, is a balanced additive system and is suited for a wide variety of machining applica..
Flash Point 182 °C
360 °F
ConocoPhillips Hydroclear® 10 Rolling Oil
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi..
Flash Point 182 °C
360 °F
ASTM D92
ChevronTexaco AFP White Oil
Chevron White Oil AFP is a technical grade white oil processed from paraffinic oilApplicationsChevron White Oil AFP’s major application is the dedusting of animal feeds and the preparation of anima..