Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | >= 40.0 °C | >= 104 °F | closed cup; ASTM D56 |
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i.. |
|||
Flash Point | 40.0 °C | 104 °F | PMCC |
Solvay CATAFOR® CA80 Surfactant Identification: QUATERNARY AMMONIUM ETHOSULPHATECAS: 68308 – 64 – 5Solubility: Readily soluble in ethyl alcohol, butanol chloroform, trichloroethylene, ethyl acetate and water.Solvent: n-B.. |
|||
Flash Point | 40.0 °C | 104 °F | |
Solvay GERONOL® FF/6 Surfactant Description: Multipurpose emulsifier for EC, to use in pair with Geronol FF/4 or Rhodacal 70/B.Identification: BLENDED EMULSIFIERSSolubility: Soluble in water and most polar and aromatic solventsAva.. |
|||
Flash Point | 40.0 °C | 104 °F | |
Solvay GERONOL® RE/70 Surfactant Description: Multipurpose emulsifier for EC formulations.Identification: BLEND OF FATTY ACIDSSolubility: Insoluble in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, E.. |