Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 5.00 °C | 41.0 °F | Setaflash, Closed Cup; ASTM D3278-82 |
Lord Adhesives Aeroglaze® 9958 Thinner Aeroglaze® 9958 thinner is used to reduce Aeroglaze primer and topcoat viscosities for spray applications.Mil-T-81772 Type IAll information provided by Lord. |
|||
Flash Point | 5.00 °C | 41.0 °F | closed cup |
Dow Corning SYL-OFF® SB 7458 COATING Base polymer component for Syl-Off® brand solvent-based, platinum-catalyzed silicone release coatingsInformation provided by Dow Corning |
|||
Flash Point | 5.00 °C | 41.0 °F | |
3M K520UV Adhesion Promoter 3M™ Adhesion Promoter K520UV is a liquid primer used to improve the adhesion of 3M™ Acrylic Foam and Acrylic Plus Tapes to Polyolefin-based substrates such as thermoplastic olefins (TPO), Polyprop.. |