Flash Point 212 °C
414 °F
ASTM D92
ExxonMobil 427 Mobilmet 400 Series
Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operation..
Flash Point 212 °C
414 °F
ASTM D92
ExxonMobil Enmist EP 100
Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist ..
Flash Point 212 °C
414 °F
ASTM D92
ExxonMobil 32 Mobil DTE FM Series
Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua..
Flash Point 212 °C
414 °F
ASTM D92
ExxonMobil Nuto 32 H Series
Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q..
Flash Point 212 °C
414 °F
ASTM D92
ChevronTexaco Mechanism LPS® ISO 68 Hydraulic Oil
Chevron Mechanism LPS Hydraulic Oils are highly refined, paraffinic oils containing oxidation and rust inhibitors, and special antiwear additives to extend the life of hydraulic pumps and motor part..
Flash Point 212 °C
414 °F
ChevronTexaco Rando® HDZ 68
Texaco Rando HDZ oils deliver value through:High oxidation stability — Longer service life than attainable with conventional lubricants used in high pressure service.Protection against rust and cor..
Flash Point 212 °C
414 °F
ASTM D92
ExxonMobil 32 Mobil DTE FM Series
Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua..
Flash Point 212 °C
414 °F
ASTM D92
ExxonMobil 427 Mobilmet 400 Series
Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operation..
Flash Point 212 °C
414 °F
ASTM D92
ExxonMobil Enmist EP 100
Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist ..
Flash Point 212 °C
414 °F
ASTM D92
ExxonMobil Mobil Velocite 10
The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydra..
Flash Point 212 °C
414 °F
ASTM D92
ExxonMobil Nuto 32 H Series
Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q..
Flash Point 212 °C
414 °F
ASTM D92
ChevronTexaco ISO 32 Turbine Oil TR
FeaturesChevron Turbine Oil TR is a premium quality turbine oil designed to meet the critical demands of bearings subjected to high temperatures.It is formulated with ISOSYN™ base stocksThis ISO 32..
Flash Point 212 °C
414 °F
Open cup
Dow Corning 5562 Carbinol Fluid
This fluid, with its carbinol functionality, has a novel compatibility profile for use in skincare, suncare, color cosmetic, and antiperspirant / deodorant applications. INCI Name: Bis-Hydroxyethoxy..
Flash Point >= 212 °C
>= 414 °F
Aremco Corr-Paint™ CP5000 High Temperature Protective Coating Inorganic, Zinc Filled
CP5000 is a two part, water-based, inorganic zinc rich primer which provides superior resistance to salt-fog, immersion, impact and abrasion. This primer system is compatible with all CP-Series prod..
Flash Point 212 °C
414 °F
ASTM D92
ChevronTexaco Rykon® ISO 68 Premium Oil
FeaturesChevron Rykon Premium Oils are designed to give maximum protection to hydraulic pumps.They are formulated with ISOSYN® base stocks incorporating antiwear additives, oxidation and corrosion ..
Flash Point 212 °C
414 °F
ASTM D92
ExxonMobil Mobil Velocite 10
The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydra..