Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 229 °C | 445 °F | |
Lubriplate AC-2A Petroleum-Based Air Compressor Fluid Formulated to reduce carbon & varnish buildup. They contain fluid zinc to effectively fight friction & wear thus reducing heat & foaming. Available in six ISO grades.AC Series Air Compressor Oils ar.. |
|||
Flash Point | 229 °C | 445 °F | |
Lubriplate H0-2A Petroleum-Based Heavy-Duty Hydraulic Oil Formulated for superior performance, this series contains fluid zinc to effectively reduce ring & vane wear. Excellent anti-rust, anti-corrosion, anti-foam and anti-oxidation properties. High anilin.. |
|||
Flash Point | 229 °C | 445 °F | |
ConocoPhillips Hydroclear Diamond Class® 68 Rotary Compressor Fluid Description: Conoco Hydroclear Diamond Class Rotary Compressor Fluids are designed to lubricate rotary screw compressors operating in air compression service. These semisynthetic products combine hi.. |
|||
Flash Point | 229 °C | 445 °F | |
ConocoPhillips Hydroclear® 1 Ultra-clean multi-purpose R&O Oil, AGMA Lubricant No. 1 Description: Conoco Hydroclear Ultra-Clean Multipurpose R&O Oil is a rust- and oxidation-inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks.. |
|||
Flash Point | 229 °C | 445 °F | |
ConocoPhillips Hydroclear® 46 Multipurpose R&O Oil, AGMA Lubricant No. 1 Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidation inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear.. |
|||
Flash Point | 229 °C | 445 °F | |
ConocoPhillips Hydroclear® 46 Turbine Oil Description: Conoco Hydroclear Turbine Oil is a premium rust- and oxidationinhibited turbine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear Turbine Oil is specially formula.. |