Flash Point 237 °C
459 °F
ASTM D92
ExxonMobil Heavy Mobil DTE Oil Named Series
The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se..
Flash Point 237 °C
459 °F
ASTM D92
ChevronTexaco Journal Bearing Oil
FeaturesChevron Journal Bearing Oil is a high quality, high viscosity index, paraffinic-based lubricant. It incorporates highly effective deposit control antioxidants and rust inhibitors as well as..
Flash Point 237 °C
459 °F
ChevronTexaco Journaltex® HD 57
Texaco Journaltex HD 57 delivers value through:Excellent lubricity characteristics imparted by the additive package minimizes friction to help prevent premature bearing failure.Good rust protection ..
Flash Point 237 °C
459 °F
ASTM D92
ExxonMobil Heavy Mobil DTE Oil Named Series
The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se..