Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 8.00 °C | 46.4 °F | |
Dow Corning A-4040 PRIME COAT Dow Corning® 9601 Textile Printing Ink is a two-component silicone product designed for manual screen printing processes. The 100:4.5 baseto- catalyst design simplifies the pigmentation process; on.. |
|||
Flash Point | 8.00 °C | 46.4 °F | closed cup |
Dow Corning Z-6070 SILANE Dow Corning Z-6070 Silane is a chemical monomer that reacts with water to form a silanetriol and methanol. The silanol that is formed is able to condense with available hydroxyl groups on the surfac.. |
|||
Flash Point | 8.00 °C | 46.4 °F | closed cup |
Dow Corning 1204 RTV PRIME COAT Clear primer in naphtha solvent for use with all one-part alcohol cure and two-part condensation cure silicone elastomersInformation provided by Dow Corning |