Polymer Property : Flash Point = 550 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 288 °C
550 °F
Average value: 288 °C Grade Count:10
Overview of materials for Styrene/Butadiene/Styrene (SBS)
This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Butadiene/Styrene (SBS)". Each property range of values reported is minimum and maximum values o..
Flash Point 288 °C
550 °F
LG Chemical LG401 Styrene-Butadiene-Styrene
Description: Radial structure, Non-Oil Extended Grade Thermoplastic ElastomerApplication: Asphalt Modifier, Plastic Modifier, Compounding, Adhesives etcCAS No. 9003-55-8Information provided by LG Ch..
Flash Point 288 °C
550 °F
LG Chemical LG-411 Styrene-Butadiene-Styrene
Description: Radial structure, Non-Oil Extended Grade Thermoplastic ElastomerApplications: Asphalt Modifier, Plastic Modifier, Compounding, Adhesives etcCAS: 9003-55-8Information provided by LG Chem..
Flash Point 288 °C
550 °F
LG Chemical LG411H Styrene-Butadiene-Styrene
Description: Radial structure, Non-Oil Extended Grade Thermoplastic ElastomerApplication: Asphalt Modifier, Compounding, Adhesives etcCAS No. 9003-55-8Information provided by LG Chemical
Flash Point 288 °C
550 °F
LG Chemical LG-428N Styrene-Butadiene-Styrene
Description: Radial structure, Non-Oil Extended Grade Thermoplastic ElastomerApplications: Asphalt Modifier, Plastic Modifier, Compounding, Adhesives etcCAS: 9003-55-8Information provided by LG Chem..
Flash Point 288 °C
550 °F
LG Chemical LG-475 Styrene-Butadiene-Styrene
Description: Radial structure, Oil Extended Grade Thermoplastic Elastomer Application: Compounding Plastic ModifierCAS: 9003-55-8Information provided by LG Chemical
Flash Point 288 °C
550 °F
LG Chemical LG-485 Styrene-Butadiene-Styrene
Description: Radial structure, Oil Extended Grade Thermoplastic ElastomerApplications: Compounding Plastic ModifierCAS: 9003-55-8Information provided by LG Chemical
Flash Point 288 °C
550 °F
Lubriplate CP-8A Petroleum-Based Gear, Bearing, & Recirculating Oil
This non-EP (Extreme Pressure) oil is manufactured with acidless tallow as required to meet AGMA specification 8A Comp. It is recommended for use in cone drives and double-enveloping worm gear drive..
Flash Point 288 °C
550 °F
Lubriplate SYN LUBE 460 PAO-Based Multi-Purpose Synthetic Fluid
PAO-based zinc free fluids formulated with state of the art additives to provide outstanding performance over extended drain intervals.Applications: Syn-Lube 150, 220, 320, 460 & 680 are recommended..
Flash Point 288 °C
550 °F
LG Chemical LG-503 Styrene-Butadiene-Styrene
Description: Linear structure, Non-Oil Extended Grade Thermoplastic ElastomerApplication: Asphalt Modifier, Plastic Modifier, Compounding, Adhesives etcCAS No. 9003-55-8Information provided by LG Ch..
Flash Point 288 °C
550 °F
ASTM D92
ExxonMobil Extra Hecta Super Mineral Mobil Cylinder Oil
Mobil Cylinder oils are extra high performance high viscosity oils designed for use in enclosed worm gears operating at moderate to high speeds and temperatures, and where heavy loads, slow speeds o..
Flash Point 288 °C
550 °F
ASTM D92
ExxonMobil Mobil Vaculine 133
The Mobil Vacuoline 100 range is a series of extra high quality circulating system oils primarily intended for the lubrication of plain bearings in systems designed for full fluid lubrication, parti..
Flash Point 288 °C
550 °F
ChevronTexaco 100 Aircraft Engine Oil
Texaco Aircraft Engine Oils deliver value through:Use of high quality straight mineral oil with low volatilityRigid quality control through production in an ISO 9002 certified facilityProvide a stab..
Flash Point 288 °C
550 °F
ASTM D92
ChevronTexaco Aero 50/Grade 100 Engine Oil AD Uncompounded
FeaturesChevron Aero Engine Oils Uncompounded are a blend of high quality base oil, with small amounts of viscosity modifier for improved fluidity at cold temperatures, antioxidant, and antifoam age..
Flash Point 288 °C
550 °F
ELM® Concrete/Asphalt WS Biodegradable Form Release Agent
Description: ELM Concrete/Asphalt Form Release WS is water soluble, biodegradable, non-toxic, stain free concrete and asphalt form release agent formulated with Biotechbased™ seed oil that permits ..
Flash Point 288 °C
550 °F
ASTM D92
ExxonMobil Extra Hecta Super Mineral Mobil Cylinder Oil
Mobil Cylinder oils are extra high performance high viscosity oils designed for use in enclosed worm gears operating at moderate to high speeds and temperatures, and where heavy loads, slow speeds o..
Flash Point 288 °C
550 °F
ASTM D92
ExxonMobil HH Mobil DTE Oil Double Letter Series
The Mobil DTE Oil Double Letter Series of lubricants are high performance heavy duty circulating oils primarily intended for continuous reuse in circulation lubrication systems for gears and bearing..
Flash Point 288 °C
550 °F
ASTM D92
ExxonMobil Mobil Vaculine 133
The Mobil Vacuoline 100 range is a series of extra high quality circulating system oils primarily intended for the lubrication of plain bearings in systems designed for full fluid lubrication, parti..
Flash Point 288 °C
550 °F
ConocoPhillips Hydroclear® 460 Multipurpose R&O Oil, AGMA Lubricant No. 7
Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear ..
Flash Point 288 °C
550 °F
ConocoPhillips Hydroclear® 460 Rolling Oil
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi..
Flash Point >= 288 °C
>= 550 °F
Open Cup
Dow Corning XIAMETER® PMCPPMX-0210 Silicone Fluid 100CS
Is chemically equivalent to DOW CORNING® 210H FLUID 100CS. This product is a heat stabilized polydimethlysiloxane, used for heat transfer.Information provided by Dow Corning
Flash Point 288 °C
550 °F
ELM® Biobased Dust Suppressant & Stabilizer
Description: ELM Biotechbased Dust Control Concentrate (DCC) is a biodegradable, non-toxic dust suppressant and stabilizer. ELM DCC is formulated with natural seed oils and proprietary emulsifiers ..
Flash Point 288 °C
550 °F
ASTM D92
ExxonMobil HH Mobil DTE Oil Double Letter Series
The Mobil DTE Oil Double Letter Series of lubricants are high performance heavy duty circulating oils primarily intended for continuous reuse in circulation lubrication systems for gears and bearing..
Flash Point 288 °C
550 °F
LG Chemical LG-512 Styrene-Butadiene-Styrene
Description: Linear structure, Non-Oil Extended Grade Thermoplastic ElastomerApplication: Asphalt Modifier, Plastic Modifier, Compounding, Adhesives etcCAS No. 9003-55-8Information provided by LG Ch..
Flash Point 288 °C
550 °F
LG Chemical LG-604 Styrene-Butadiene-Styrene
Description: Linear structure, Non-Oil Extended Grade Thermoplastic ElastomerApplication: Asphalt Modifier, Plastic Modifier, Compounding, Adhesives etcCAS No. 9003-55-8Information provided by LG Ch..
Flash Point 288 °C
550 °F
ASTM D92
ChevronTexaco ISO 220 Cylinder Oil W
FeaturesChevron Cylinder Oils W are designed to meet the needs of emulsifying cylinder oils.Chevron Cylinder Oils W provide excellent metal wettability. The combination of oil emulsibility and metal..
Flash Point 288 °C
550 °F
LG Chemical LG-501 Styrene-Butadiene-Styrene
Description: Linear structure, Non-Oil Extended Grade Thermoplastic ElastomerApplication: Asphalt Modifier, Plastic Modifier, Compounding, Adhesives etcCAS No. 9003-55-8Information provided by LG Ch..