Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | >= 302 °C | >= 575 °F | ASTM D 92 |
ConocoPhillips 460 Bearing Oil Description: Conoco Bearing Oil is formulated for the circulating systems that lubricate roll-neck bearings in steel and nonferrous rolling mills. It is suited for systems in which water and corrosi.. |