Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 320 - 340 °C
608 - 644 °F
LG Chemical LK170 PVC
General Description: LK170, vinyl chloride copolymer with vinyl acetate exhibit excellent properties including easy processing and effective flowMain Applications: Sealant, automotive protective sol..