Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | >= 61.0 °C | >= 142 °F | |
Solvay GERONOL® FF/4-E Surfactant Description: Multipurpose emulsifier for agrochemical formulations. Used in pair with Geronol FF/6-C or MS-C.Identification: BLENDED EMULSIFIERSSolubility: Dispersible in water. Soluble in most pola.. |
|||
Flash Point | >= 61.0 °C | >= 142 °F | |
Solvay GERONOL® FF/6-E Surfactant Description: Multipurpose emulsifier for EC, to use in pair with Geronol FF/4 or Rhodacal 70/B.Identification: BLENDED EMULSIFIERSSolubility: Dispersible in water. Soluble in most polar and aromatic.. |
|||
Flash Point | >= 61.0 °C | >= 142 °F | |
Solvay GERONOL® TE 300 Surfactant Description: Emulsifier for agrochemical formulations.Identification: BLENDED EMULSIFIERSSolubility: Dispersible in water. Soluble in most polar and aromatic solventsAvailable in: Asia Pacific, Euro.. |
|||
Flash Point | >= 61.0 °C | >= 142 °F | |
Solvay RHODACAL® 60/BE Surfactant Description Anionic, high flash point, linear Calcium dodecylbenzene sulfonate, 60% active , useful in emulsifier blends where high flash point is required.Identification: LINEAR DODECYLBENZENE SULP.. |
|||
Flash Point | >= 61.0 °C | >= 142 °F | Closed cup |
Dow Corning Q2-5247 Fluid Surface active silicone designed for reducing surface tension in silicone emulsions and improving drainage in pulp brownstock washing.Information provided by Dow Corning |
|||
Flash Point | 61.0 °C | 142 °F | closed cup |
Dow Corning Z-6376 SILANE Chloropropyltriethoxysilane - Used to pretreat or be added to the resin for integral treatment. Improves chemical bonding of resins to inorganic materials.Information provided by Dow Corning |
|||
Flash Point | >= 61.0 °C | >= 142 °F | |
Solvay RHODISOLV® GREEN 21 Solvent Identification: BLEND OF SOLVENTSAvailable in: Asia Pacific, Europe, Latin America and North AmericaSolubility: Insoluble in water. Soluble in most polar and aromatic solvents. Applications: Solvent.. |
|||
Flash Point | >= 61.0 °C | >= 142 °F | |
Solvay RHODISOLV® GREEN 25 Solvent Identification: BLEND OF SOLVENTSAvailable in: Asia Pacific, Europe, Latin America and North AmericaSolubility: Insoluble in water. Soluble in most polar and aromatic solvents. Applications: Solvent.. |