Thermal Properties Metric English Comments
Flash Point 66.0 °C
151 °F
closed cup
Dow Corning SYL-OFF® 7048 CROSSLINKER
Syl-Off® 7048 Crosslinker is a 100% active solids silicone crosslinker. Recommended where optimum anchorage to substrate is required. Suitable for use with most Syl-Off® Solventless and Solvent ba..
Flash Point 66.0 °C
151 °F
Closed cup
Dow Corning SYL-OFF® PMCP7048 Crosslinker
Syl-Off® 7048 Crosslinker is a 100% active solids silicone crosslinker. Recommended where optimum anchorage to substrate is required. Suitable for use with most Syl-Off® Solventless and Solvent ba..
Flash Point 66.0 °C
151 °F
As Received; ASTM D93, DIN 51 755
Chesterton 775 Moisture Shield
Description: Chesterton® 775 Moisture Shield is a moisture displacing, clear protective coating that protects parts and equipment from corrosion for months. Sprayed on bare metal, it leaves a lubri..