Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 92.8 °C | 199 °F | HPC-3 Curative; Seta |
Lord Adhesives HPC-3C Fluoroelastomer Coating LORD HPC-3B and HPC-3C are two-part, room temperature curing fluoroelastomer coatings which feature robust adhesion and exceptional mechanical properties. These coatings greatly enhance fuel and flu.. |
|||
Flash Point | 92.8 °C | 199 °F | HPC-3 Curative; Seta |
Lord Adhesives HPC-3B Fluoroelastomer Coating LORD HPC-3B and HPC-3C are two-part, room temperature curing fluoroelastomer coatings which feature robust adhesion and exceptional mechanical properties. These coatings greatly enhance fuel and flu.. |
|||
Flash Point | 92.8 °C | 199 °F | Method A; ASTM D93 |
ExxonMobil Exxsol™ D220/240 Dearomatized Fluid Availability: Africa & Middle East, Europe, Central America and South America Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |