Thermal Properties Metric English Comments
Decomposition Temperature 372 °C
702 °F
Degradation Temperature
Epoxy Technology EPO-TEK® H20-HC Electrically Conductive Epoxy
Product Description: EPO-TEK® H20E-HC is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is al..
Decomposition Temperature 372 °C
702 °F
Degradation Temperature
Epoxy Technology EPO-TEK® H35-175MP Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H35-175MP is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-elec..
Decomposition Temperature 372 °C
702 °F
Degradation Temperature; TGA
Epoxy Technology EPO-TEK® E3035 Electrically Conductive Adhesive
Product Description: EPO-TEK® E3035 is a single component, silver-filled epoxy for hybrid die and component attach.Advantages & Application Notes: Performs exceptionally well as a die attach for sm..