Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 350 - 380 °C | 662 - 716 °F | ASTM E1131 |
Zeus ETFE Tubing ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess.. |