Polymer Property : Decomposition Temperature = 392 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature 190 - 200 °C
374 - 392 °F
Polimeros Mexicanos Rotofoam® Plus 93050 Medium Density Polyethylene, Foam Grade
Hexene Copolymer Linear Medium Density Polyethylene for foaming applications. It is formulated for inner layers with excellent foam cell structure and smooth surface finish and uniform closed cells...
Decomposition Temperature 185 - 200 °C
365 - 392 °F
Average value: 188 °C Grade Count:5
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..