Polymer Property : Decomposition Temperature = 487 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature 487 °C
909 °F
Degradation Temperature
Epoxy Technology EPO-TEK® 354 High Temperature Epoxy
Product Description: EPO-TEK® 354 is a two component, high Tg epoxy designed for semiconductor packaging in medical, fiber optic and optoelectronic assemblies. It is an electrically and thermally i..
Decomposition Temperature 487 °C
909 °F
Onset; IPC TM-650 2.4.24.6
Arlon CLTE-AT Commercial Ceramic PTFE
Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-AT is a micro-dispersed ceramic PTFE composite utilizing ..