Thermal Properties Metric English Comments
Decomposition Temperature 322 °C
612 °F
Onset; IPC TM-650 2.3.41
Arlon 37N Polyimide Low-Flow
37N is a polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow is requir..