Polymer Property : Decomposition Temperature = 714 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature 379 °C
714 °F
Degradation Temperature
Epoxy Technology EPO-TEK® P1011S Electrically Conductive Modified Polyimide
Product Description: EPO-TEK® P1011S is a single component, modified polyimide, high temperature grade, silver-filled electrically and thermally conductive adhesive designed for semiconductor die-a..