Polymer Property : Decomposition Temperature = 750 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature 399 °C
750 °F
Degradation Temperature
Epoxy Technology EPO-TEK® H54 High Temperature Epoxy
Product Description: EPO-TEK® H54 is a two component, high Tg, electrically and thermally insulating epoxy adhesive for general bonding and high temperature packaging in medical, hybrid, and optica..