Polymer Property : Decomposition Temperature = 853 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature 456 °C
853 °F
Degradation Temperature
Epoxy Technology EPO-TEK® H31D-LV Epoxy
Material Description: A single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and optoelectronic packaging. It i..
Decomposition Temperature 456 °C
853 °F
Degradation Temperature
Epoxy Technology EPO-TEK® OE101 Two Component Epoxy
Material Description: A two component epoxy designed for low stress applications in fiber optic packaging, opto-electronics and semiconductors. It is a lower modulus version of EPO-TEK® 353ND.Inf..