Thermal Properties | Metric | English | Comments |
---|---|---|---|
Smoke Density | 1.50 - 50.0 min | 1.50 - 50.0 min | Average value: 15.3 min Grade Count:15 |
Overview of materials for Silicone Foam This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatW.. |