Thermal Properties Metric English Comments
Flame Spread 2.00 mm/min
0.0787 in/min
FMVSS 302
SABIC Innovative Plastics LNP Thermocomp RF006XXP PA 66 (Europe-Africa-Middle East)
30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.