Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flame Spread = 0.35 in/min Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flame Spread 9.0 mm/min
0.35 in/min
FMVSS302
Polyram RamOfin PPH301G6NT Polypropylene, 30% Glass Fiber
30% Glass fiber reinforced polypropylene for injection molding applications. Approved and listed by WRAS Potable Water.Information provided by Polyram.