Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 20 mm/min | 0.79 in/min | Automotive Burn Test; FMVSS 302 |
PolyOne Geon™ Vinyl Flexible 90463 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Flame Spread | 20 mm/min | 0.79 in/min | FMVSS302 |
Polyram Polytron P50B07 Polypropylene, 50% Long Glass Fiber, UV Stabilized A chemically coupled 50% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Flame Spread | 20 mm/min | 0.79 in/min | FMVSS302 |
Polyram PlusTek PB826G3 Nylon 6 for Injection Molding, 15% Glass-fiber Reinforced, Impact Modified and UV Stabilized 15% Glass fiber reinforced, impact modified and UV stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |