Polymer Property : Flame Spread = 0.80 in/min Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flame Spread 20 mm/min
0.80 in/min
Burning Rate UL 94 HB; ASTM D635
Spartech Polycast Poly 76 (Mil-P-8184) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flame Spread 20 mm/min
0.80 in/min
Burning Rate UL 94 HB; ASTM D635
Spartech Polycast Poly 84 (Mil-P-8184) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Flame Spread 20 mm/min
0.80 in/min
Horizontal Burn Rate; FMVSS302
Asahi Kasei Thermofil P-20TC-1156 20% Talc Filled, Heat Stabilized
Information provided by Asahi Thermofil
Flame Spread 20 mm/min
0.80 in/min
Horizontal Burn Rate; FMVSS302
Asahi Kasei Thermofil P-20TC-5103 20% Talc Reinforced, Lubricated, Heat Stabilized
Information provided by Asahi Thermofil
Flame Spread 20 mm/min
0.80 in/min
Horizontal Burn Rate; FMVSS302
Asahi Kasei Thermofil P-40TC-8100 40% Talc Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flame Spread 20 mm/min
0.80 in/min
Horizontal Burn Rate; FMVSS302
Asahi Kasei Thermylene® P6-30FG-0600 30% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil